Features
- DCT is manufactured with radiation crosslinked polyolefin
- Specially developed chemical formulation makes the tubing provide effective insulation screen on the high voltage cable connectors
- Minimum shrink temperature: 100oC
- Minimum fully recovered temperature:1200C
Technical Data (For inner layer)
| Property |
Requirements |
Test Method |
| Operating temperature |
-45oC to +100oC |
IEC 216 |
| Tensile strength |
8N/mm2 (min.) |
|
| Elongation at break |
200 % min |
ASTM D 638 |
| Water absorption |
1% max |
ASTM D 638 |
| Elongation at break after aging |
150% (min.) |
150oC, 168 hrs. |
| Volume resistance |
104 .cm |
IEC 93 |
| Longitudinal shrinkage |
±10% |
-- |
| Eccentricity |
<40% |
ASTM D 2671 |
Dimension Chart
| Code |
Diameter |
Recovered Wall thinkness W (mm) |
|
| D1(max. in mm) |
D2(min. in mm) |
| DCT - 30/12 |
30 |
12 |
2.5 |
Enquiry |
| DCT - 35/12 |
35 |
12 |
2.5 |
Enquiry |
| DCT - 40/14 |
40 |
14 |
2.5 |
Enquiry |
| DCT - 45/14 |
45 |
14 |
2.5 |
Enquiry |
| DCT - 50/18 |
50 |
18 |
2.5 |
Enquiry |
| DCT - 55/18 |
55 |
18 |
2.5 |
Enquiry |
| DCT - 60/20 |
60 |
20 |
2.5 |
Enquiry |
| DCT - 65/20 |
65 |
20 |
2.5 |
Enquiry |
| DCT - 70/20 |
70 |
20 |
2.5 |
Enquiry |
| DCT - 80/28 |
80 |
28 |
3.0 |
Enquiry |
|